Show solutionHide solution
Question 10
Correct a crystallinity calculation for cold crystallization and filler
Use the specified model for initial polymer crystallinity: . The filler is inert, and the reference applies to the same crystal form.
Diagram shown in the original SVG worksheet.
Calculate initial crystallinity of the polymer fraction.
Explain why the cold-crystallization enthalpy is subtracted.
What incorrect value results if filler normalization is omitted?
Question 10 - Solution
Correct a crystallinity calculation for cold crystallization and filler
Diagram shown in the original SVG worksheet.
(a)
Xc = (60-20)/(0.80 times 200) = 0.25, or 25 percent of the polymer fraction.
(b)
Crystals formed during heating contribute to the later melting peak but were absent initially. Subtraction removes that contribution in this model.
(c)
Omitting the polymer mass fraction gives 40/200 = 0.20, or 20 percent; this uses the whole-sample mass basis incorrectly.